Mirror Lip Glaze 20230210BA01


Procedure

1. Add part A into the vessel 1 and heat to 60-65℃ with stirring until the solid dissolved and then add pre-mixed part B into the vessel until uniform. 2. Add part C into the vessel 2 and heat to 100-110℃ with stirring until transparent, and then cool down to 65-70℃ add part D into vessel 2 with stirring until uniform. 3. Add part C and part D into the vessel 1 with stirring until uniform and homogenize for 3-5 minutes. 4. Cool down to 40-45℃, add part E into the vessel with stirring until uniform. 5. Testing and packing.